Calling on the wisdom of Marq, Charger, or whomever...
On my test panel, I am using Rusto and am to the point that the formerly brown panel is now definitely red. Paint is thin, following the "roll it in the pan" to squeeze excess off before "wetting" the panel with paint. That seems to work very well for me as far as getting the paint to flow out so I don't get roller marks. But, the paint is drying with a more matte finish, it's not glossy like it would be if I brushed it on very thick and just left it to dry, brush marks and all (It's glossier from where it drips down the side of the can than it is on my test door). My theory is that I still don't have enough layers of paint so either 1. I just need more thickness for it to gloss or 2. I am still seeing the matte finish from where I wetsanded the coat below it. What say those with more experience?

Last edited by tett; 07/27/07 09:59 PM.