Quote:

Ok, now a few insights:

1.) The paint suggested very early in these postings was called "acrylic/enamel paint"...this is not exactly what you're looking for. The proper paint type is "aklyd enamel". The "acrylic/enamel" is water based, and that isn't what you want (read about "acrylic/enamel" on this web page). As a matter of fact, you do not necessarily have to buy "rustoleum". I bought mine from the local "Do-It-Center" and it is the house brand made by Sherwin Williams...worked fine. The easiest way to tell if you have the right thing is to look at the directions and see what "clean-up" instructions are...if it says "clean with Mineral Spirits", than you have the right stuff. Many people make compatible brands.

2.) It may also say in the instructions that you do not have to thin...in this case, you have to thin. My ratio was 10:1, worked great. It will bubble and look "orange peely" at first, but relax, the paint self-levels as it drys.

3.) At first, I understood that we could use a $20 orbital buffer/polisher like you buy a Wal-Mart, etc...Although it seems to have worked for others, it did NOT work for me. It would not eliminate the scratches from the final 1500 grit wetsanding. Luckily, I had a 7" ELECTRONIC POLISHER/SANDER just like the one on this web page. It worked wonders!!

Will write more later if I think of anything. If you have questions about my procedure, I will do my best to help...thanks guys




i allways have suggested the alklyd enamel (rust paint) to roller on, i think the confusion comes from the 71 midnight metalic blue beetle in my pics that was SPRAYED with dupli color single stage acrylic enamel. just to clear things up.

by the way, nice job, i hope to see it all done