Quote:

Thanks guys, but the method is to do away with ANY orange peel before the next coat, correct?




My understanding is you put on 2 coats rustoleum/tremclad (1 for brightside), let it dry and then remove any blemishes, orange peel, dust, fibers, etc, then 2 more coats, and repeat, with successively finer sand paper grits finishing with something like 1500 or 2000 grit on the final coat (6th+ coat possibly as much as the 10th apparently or 3rd or 4th with brightside). Then polish/buff until it shines like you want, then cure another day or three and wax the shine into place.