Originally Posted by 73cuda340
I ended up getting the flares to come out nice. The trick was, as recommended , to heat the tubing up, and then quickly flare it. I just finished the rear axle and all of the flares ended up looking nice. Thanks for the help.


I would suggest to check on the effects of heating the stainless and its result. Just to make sure its not to brittle or soft. there are different grades of SS and I for one am not sure of the lasting effects of doing so on any of the grades. Might be OK, Might not shruggy wink :beer