Originally Posted by Cab_Burge

Molnars ARP 2000 bolts are different also and you can NOT buy them directly from ARP work shruggy
Does MGP make and steel steel rods or aluminum only?


I didn't know that about the Molnar rod bolts.

MGP only makes aluminum rods that I'm aware of. I'm going aluminum because I may have reached the limit of a steel rod with a blower. I haven't had an issue with detonation is the reason I used the steel rod.
And, other than Oliver I don't know of any other manufacturer who's rods will handle up to 2000 HP. I'm sure there are some however.
I really haven't researched a steel rod under power adder conditions that much, at the time I got the Oliver's I was running NA.
I don't like the idea of changing out the rods often, but...... shruggy Not to mention it's hard to get a intelligent answer on how many runs I can reasonably expect. I'm told 50-1000 by different people


Dave
.