I did some lead work on some pitted metal today and was pretty impressed with the result. I know it's a dying art but was interested in hearing others opinion's on the use of it. Which method do you prefer, Lead or Bondo and why? I'm interested in hearing the pros and cons of each as well as the best application to use them in. Thoughts? work