Jim, the foam used to make those gaskets was formed inside a mold so the chemicals were injected, blended, and cured against the side walls of the molds which effectively made the outer skin that contacted the walls a closed cell appearance. The foam itself was quite soft and spongy durometer wise, and had a very fine open cell size.