Quote:

Even after blasting if you preheat the parts it burns the contaminates out of the pores.




That makes since.

So should you heat the parts for a while to get the contaminates all out? Last time I just put them in long enough to get the part hot; Like 5 minutes.

Just seem the cheap Kylon type paints do not go on very good anymore. Very fustrating.